What must be done if the concrete drops below the top of the Slump mold while the top
layer is being rodded?
Add additional concrete to keep an excess of concrete above the top of the mold at all
times
Rod each layer ___ times uniformly over the cross section with the rounded end of the
rod.
25
The slump mold is filled in _____ layers.
3 layers
True or false the slump mold should be in a dry condition before beginning the test?
False.
For use in the slump test, the tamping end on both ends of the tamping rod must be...
Rounded to a hemispherical tip
True or false the Anterior surface of the slump mold is allowed to have minor
irregularities?
False
The mold for making the slump test is in the shape of
The frustum of a cone
What is the maximum allowable time between obtaining the first and final portion of the
composite samples?
15 minutes
True or false the sample of concrete used for temperature determination must be
rodded 25 time?
False
What is the required shape of the tamping end of the tamping rod?
Rounded to a hemispherical tip